Industrial metal background

HASTELLOY Alloy 6-3 Plate/Sheet

特殊合金板材
UNS N06985 sheet

概述

HASTELLOY Alloy 6-3 (UNS N06985) is a nickel-chromium-molybdenum-copper superalloy containing Ni bal, Cr 22, Fe 19.5, Mo 7, Cu 1.9, and Co 5 max, designed for exceptional resistance to sulfuric acid and oxidizing chloride environments. The higher molybdenum content (7) and copper addition (1.9) compared to HASTELLOY 6 provide improved resistance to reducing acids, while the controlled cobalt content enhances structural stability. The alloy is widely used in chemical process equipment for handling sulfuric acid, hydrochloric acid mixtures, and other aggressive media.

描述(英文)

HASTELLOY Alloy 6-3 is supplied in the sheet solution heat-treated condition, delivering yield strength of 324 MPa, tensile strength of 690 MPa, elongation of 50%, and hardness of HRB 79. The alloy is manufactured to multiple ASTM standards covering sheet/plate/strip (B 582), rod (B 581), pipe and tube (B 619, B 622, B 626), and fittings (B 366). The good ductility (50%) combined with high chromium and molybdenum content makes the alloy suitable for welded fabrications in the chemical process industry. HASTELLOY 6-3 is widely used in chemical processing, fertilizer production, and marine applications.

尺寸范围

  • Sheet: 0.5 - 6 mm thickness, Width up to 1200 mm, Length up to 3000 mm
  • Plate: 6 - 50 mm thickness, Width up to 1500 mm, Length up to 3000 mm
  • Strip: 0.1 - 3 mm thickness, Width up to 300 mm, Coil

牌号标准

标准体系数值
🇺🇸 ASTMB 434
EuropeanEN 10095, DIN 17750
ChinaGB/T 15007, GB/T 2054
JapanJIS H4551
AerospaceAMS

化学成分

元素数值
Cr22
Mo7
Fe19.5
Mn0.8
Si0.4
Cb+Ta0.3
W1.5Max
Cu1.9
Co5Max
C0.015max
Nibal

机械性能

productCenter.property数值
Yield Strength (0.2% offset)324 MPa
Tensile Strength690 MPa
Elongation (in 2 in)50%
HardnessHRB 79

物理性能

性能单位数值
Densityg/cm³0.316 lb/cu in
Specific Gravity-8.75
Melting Point°C2480 °F
Specific Heat (32-212°F)J/kg·K0.105 Btu/lb/°F
Thermal Expansion Coefficient (32-212°F)×10⁻⁶/K6.8 in/in/°F × 10⁻⁶
Thermal Conductivity (32-212°F)W/m·K75 Btu/sq ft/hr/°F/in
Electrical Resistivity (68°F)μΩ·cm 695 ohms/cir mil ft
Tensile Modulus of ElasticityGPa29.5 × 10⁶ psi