713C镍基高温合金带卷具有良好的高温强度、抗氧化性能和抗热疲劳性能。供应商目录列出的厚度范围为0.03–16.0 mm,最大宽度为1,200 mm。具体供货形式及性能需以实际产品标准和材质证明为准。
尺寸范围
- Thickness: 0.03–16.0 mm
- Width: Up to 1,200 mm
- Coil Inner Diameter: To be confirmed
- Coil Outer Diameter: To be confirmed
- Coil Weight: To be confirmed
牌号标准
| 标准体系 | 数值 |
|---|---|
| Alloy 713C | - |
| IN-713C | - |
| 2.4671 | - |
化学成分
| 元素 | 数值 |
|---|---|
| Nickel (Ni) | Balance, approximately 74% |
| Chromium (Cr) | 12.00–14.00% |
| Molybdenum (Mo) | 3.80–5.20% |
| Niobium + Tantalum (Nb + Ta) | 1.80–2.80% |
| Aluminum (Al) | 5.50–6.50% |
| Titanium (Ti) | 0.50–1.00% |
| Carbon (C) | 0.08–0.20% |
| Boron (B) | 0.005–0.015% |
| Zirconium (Zr) | 0.05–0.15% |
机械性能
| 性能 | 数值 |
|---|---|
| 0.2% Yield Strength | ≥ 690 MPa |
| Tensile Strength | ≥ 758 MPa |
| Elongation | ≥ 3% |
| Hardness | 30–42 HRC |
| Stress-Rupture Life | ≥ 30 hours at 982°C under 152 MPa |
| Stress-Rupture Elongation | ≥ 5% |
物理性能
| 性能 | 单位 | 数值 |
|---|---|---|
| Density | - | 7.91 g/cm³ |
| Melting Range | °C | 1,260–1,288 |
应用场景
- High-temperature industrial components
- Turbine components
- Heat-resistant cast components