合金钢板材Configure in CMSAlloy 713C

产品描述
Alloy 713C是一种镍基沉淀强化高温合金,具有良好的高温强度、抗氧化性能和抗热疲劳性能,适用于高温工业部件。具体产品形态、尺寸及性能以适用标准和供应商材质证明为准。
尺寸范围
- Thickness: 2–25 mm (precision-cast plate, supplier-listed range)
- Width: 200–500 mm
- Length: 500–1,000 mm
- Custom Dimensions: Available upon requestYield Strength: ≥ 690 MPa
牌号标准
| 标准体系 | 数值 |
|---|---|
| Alloy 713C | - |
| IN-713C | - |
化学成分
| 元素 | 数值 |
|---|---|
| Chromium (Cr) | 12–14% |
| Molybdenum (Mo) | 3.8–5.2% |
| Aluminum (Al) | 5.5–6.5% |
| Titanium (Ti) | 0.5–1.0% |
| Nickel (Ni) | Balance |
机械性能
| 性能 | 数值 |
|---|---|
| Yield Strength | ≥ 690 MPa |
| Tensile Strength | ≥ 760 MPa |
| Elongation | ≥ 3% |
| Hardness | 30–42 HRC |
| Stress-Rupture Life | ≥ 30 hours at 982°C under 152 MPa stress, with ≥ 5% elongation |
物理性能
| 性能 | 单位 | 数值 |
|---|---|---|
| Density | - | Approximately 7.91 g/cm³ |
| Melting Range | - | Approximately 1,260–1,288°C |
应用场景
- Gas turbine components
- High-temperature castings
- Industrial thermal equipment
- Heat-resistant components
- Specialized high-temperature machinery