Description (English)

HASTELLOY Alloy C-4 is supplied in the sheet solution heat-treated condition, delivering yield strength of 414 MPa, tensile strength of 765 MPa, elongation of 52%, and hardness of HRB 90. The alloy is manufactured to multiple ASTM standards covering plate/sheet/strip (B 575), rod (B 574), pipe and tube (B 619, B 622, B 626), and fittings (B 366). The titanium stabilization minimizes the formation of grain boundary carbides during thermal cycling, ensuring that corrosion resistance is maintained in welded and high-temperature-exposed conditions. HASTELLOY C-4 is widely used in the chemical process industry for heat exchangers, reactors, columns, and piping systems handling aggressive chemicals.

Size Range

  • sheet:thickness:0.5-6mm,width:up to 1200mm,lenth:3000mm
  • plate:thickness:6-50mm,width:up to 2000mm,lenth:6000mm

Grade Specification

SystemValue
🇺🇸 UNSN06455
🇪🇺 ENNiMo16Cr16Ti / 2.4610
🇩🇪 DIN2.4610
AFNORNiMo16Cr16Ti
🇨🇳 GBNS335
🇯🇵 JISNW6455

Chemical Composition

ElementValue
NiBal
Cr16
Mo15.5
Fe3max
Co2max
Mn1max
Ti0.70max
Si0.08max
C0.015max

Mechanical Properties

PropertyValue
• Yield Strength414 MPa
• Tensile Strength765 MPa
• Elongation (in 2 in)52%
• HardnessHRB 90

Physical Properties

PropertyUnitValue
Density-8.64g/cm³
Melting Range°C1335 - 1380℃
Thermal Conductivity (20°C)-10.0W/m·K
Electrical Resistivity (20°C)-135µΩ·cm
Specific Heat Capacity (20°C)-400 J/kg·K
Thermal Expansion Coefficient (20-100°C)-10.8×10⁻⁶/K
Modulus of Elasticity (20°C)-211GPa

Applications

  • • Wet-process phosphoric acid equipment
  • • Sulfuric acid heat exchangers and reactors
  • • Chemical process columns and vessels
  • • Piping systems for aggressive media
  • • Fertilizer production equipment
  • • Pulp and paper digesters
  • • Flue gas handling systems
  • • Pharmaceutical processing equipment