Description (English)

Alloy 713C nickel-based superalloy strip coil offers high-temperature strength, oxidation resistance, and thermal fatigue resistance. Supplier-listed dimensions range from 0.03 to 16.0 mm in thickness, with widths up to 1,200 mm. Actual availability and mechanical properties depend on the manufacturing process and material specification.

Size Range

  • Thickness: 0.03–16.0 mm
  • Width: Up to 1,200 mm
  • Coil Inner Diameter: To be confirmed
  • Coil Outer Diameter: To be confirmed
  • Coil Weight: To be confirmed

Grade Specification

SystemValue
Alloy 713C-
IN-713C-
2.4671-

Chemical Composition

ElementValue
Nickel (Ni)Balance, approximately 74%
Chromium (Cr)12.00–14.00%
Molybdenum (Mo)3.80–5.20%
Niobium + Tantalum (Nb + Ta)1.80–2.80%
Aluminum (Al)5.50–6.50%
Titanium (Ti)0.50–1.00%
Carbon (C)0.08–0.20%
Boron (B)0.005–0.015%
Zirconium (Zr)0.05–0.15%

Mechanical Properties

PropertyValue
0.2% Yield Strength≥ 690 MPa
Tensile Strength ≥ 758 MPa
Elongation ≥ 3%
Hardness30–42 HRC
Stress-Rupture Life≥ 30 hours at 982°C under 152 MPa
Stress-Rupture Elongation≥ 5%

Physical Properties

PropertyUnitValue
Density- 7.91 g/cm³
Melting Range°C 1,260–1,288

Applications

  • High-temperature industrial components
  • Turbine components
  • Heat-resistant cast components
  • Specialized thermal equipment