Alloy 713C Sheet & Plate | IN-713C Superalloy

Alloy SteelSheet/PlateConfigure in CMSAlloy 713C
713Cι•εŸΊι«˜ζΈ©εˆι‡‘ζΏ
1/5

Description (English)

Alloy 713C, also known as IN-713C, is a precipitation-hardenable nickel-based superalloy designed for high-temperature applications. It offers high-temperature strength, oxidation resistance, and thermal fatigue resistance. Product dimensions, availability, and mechanical properties depend on the applicable specification and manufacturing process.

Size Range

  • Thickness: 2–25 mm (precision-cast plate, supplier-listed range)
  • Width: 200–500 mm
  • Length: 500–1,000 mm
  • Custom Dimensions: Available upon requestYield Strength: β‰₯ 690 MPa

Grade Specification

SystemValue
Alloy 713C-
IN-713C-

Chemical Composition

ElementValue
Chromium (Cr)12–14%
Molybdenum (Mo)3.8–5.2%
Aluminum (Al)5.5–6.5%
Titanium (Ti)0.5–1.0%
Nickel (Ni)Balance

Mechanical Properties

PropertyValue
Yield Strength β‰₯ 690 MPa
Tensile Strengthβ‰₯ 760 MPa
Elongation β‰₯ 3%
Hardness 30–42 HRC
Stress-Rupture Lifeβ‰₯ 30 hours at 982Β°C under 152 MPa stress, with β‰₯ 5% elongation

Physical Properties

PropertyUnitValue
Density-Approximately 7.91 g/cmΒ³
Melting Range-Approximately 1,260–1,288Β°C

Applications

  • Gas turbine components
  • High-temperature castings
  • Industrial thermal equipment
  • Heat-resistant components
  • Specialized high-temperature machinery